IMP HOME
STAFF
MECHANICAL ALLOYING

Consolidation Processing


  • Workpieces up to 175 mm in diameter can be hot isostatically pressed at:
    • Pressures up to 517 MPa (75,000 psi)
    • Temperatures up to 1300o C
  • Materials can also be consolidated by:
    • Vacuum sintering (to 1650oC)
    • Overpressure sintering
    • Vacuum hot pressing
High Pressure HIP